Research Article

Durability Studies on Fly Ash Based Geopolymer Concrete Incorporated with Slag and Alkali Solutions

Table 6

Weight loss in percentage of the geopolymer and OPC concrete mix after sulphate test for different curing periods.

Mix ID28 days56 days90 days

OPC0.7780.8551.063
GC10.9921.0761.218
GC21.0401.1241.306
GC31.1651.1891.391