Research Article
Electroosmotic Dewatering of Iron Ore Tailings: A Laboratory Study to Improve Geotechnical Properties
Table 1
Characteristics of analyzed iron ore tailings.
| Property | Value |
| Dry density (g/cm3) | 1.49 | Wet density (g/cm3) | 2.34 | Mineralogical composition | Magnetite, quartz, zeolite, and iron complex compounds | Chemical composition | Ti % 0.72, Si % 1.46, Fe % 61.30, Mg 1.0%, % Al 0.87 and C % 4.21 | Particle size (µm) | Dv10: 9.81; Dv50: 47.0, Dv90: 146 | Specific surface area (m2/kg) | 341.9 | Atterberg limits | The liquid limit is 25%, plastic limit is 18.75%, and the plasticity index is 6.25 low plastic material | pH | 8.2 | Water content (%) | 56.99 |
|
|