Research Article

An Experimental Study on the Lateral Stress of Composite Steel Wall Structure by Using Self-Compacting Concrete

Figure 9

Measured lateral stress loaded on the steel plate with different concrete heights. (a) Lateral stress when pouring height is 5 m. (b) Lateral stress when pouring height is 5.5 m. (c) Lateral stress when pouring height is 6 m. (d) Lateral stress when pouring height is 6.5 m. (e) Lateral stress when pouring height is 7.5 m. (f) Lateral stress when pouring height is 8.5 m.
(a)
(b)
(c)
(d)
(e)
(f)