Research Article
Effect of Elevated Temperature on the Properties of Self-Compacting Mortar Containing Nanomaterials and Zircon Sand
Table 3
Mortar specimen details for each test.
| | Experiments | Codal provision/standard | Details of the specimen |
| | Strength tests | | Compressive strength | IS 516: 1959 | 150 mm cube | | Flexural strength | IS 516: 1959 | 500 × 100 × 100 mm prism | | Ultrasonic pulse velocity | IS 13311-I: 1992 | 150 mm cube | | Durability tests | | Water absorption | ASTM C-642 | 50 mm thick × 100 mm dia | | Porosity | ASTM C-642 | 50 mm thick × 100 mm dia | | Electrical resistivity | — | 50 mm thick × 100 mm dia | | RCPT | ASTM C1202-1995 | 50 mm thick × 100 mm dia | | RCMT | NT-build 492 1999 | 50 mm thick × 100 mm dia | | Bulk diffusion | ASTM C 1556 | 50 mm thick × 100 mm dia | | Microstructure | | SEM | — | Broken powdered specimens | | XRD | — | Broken powdered specimens | | FTIR | — | Broken powdered specimens |
|
|