Research Article
Preparation, Encapsulation, and Performance Evaluation of Ternary Phase Change Materials for Building Envelope
Table 1
Changes of mass and loss rate of phase change expanded perlite under different encapsulation methods.
| Cycle number | 0 | 10 | 20 | 30 | 40 | 50 | Packaging materials | Unencapsulate | Mass/g | 20.00 | 19.73 | 19.37 | 19.12 | 18.98 | 18.98 | Loss rate/% | 0 | 1.4 | 3.2 | 4.4 | 5.1 | 5.1 |
| Styrene-acrylic emulsion | Mass/g | 39.52 | 39.34 | 39.2.4 | 39.16 | 39.16 | 39.16 | Loss rate/% | 0 | 0.9 | 1.7 | 1.8 | 1.8 | 1.8 |
| Cement powder | Mass/g | 39.27 | 39.05 | 38.95 | 38.87 | 38.85 | 38.85 | Loss rate/% | 0 | 1.1 | 1.6 | 2.0 | 2.1 | 2.1 |
| Styrene-acrylic emulsion and cement powder | Mass/g | 49.61 | 49.52 | 49.49 | 49.48 | 49.48 | 49.48 | Loss rate/% | 0 | 0.44 | 0.60 | 0.65 | 0.65 | 0.65 |
|
|