Basic physical parameters of intact samples.
| Temperature/°C | Specimen number | Before heating | After heating | Diameter (mm) | Height (mm) | Quality (g) | Diameter (mm) | Height (mm) | Quality (g) |
| 25 | DJ02-01 | 50.04 | 24.95 | 125.81 | Unheated | DJ02-02 | 50.05 | 24.92 | 122.17 |
| 100 | DJ02-07 | 50.08 | 24.92 | 125.82 | 50.07 | 24.96 | 124.15 | DJ02-08 | 50.08 | 24.91 | 125.48 | 50.11 | 24.92 | 123.70 |
| 200 | DJ02-09 | 50.06 | 24.91 | 125.21 | 50.05 | 24.96 | 120.68 | DJ02-10 | 50.03 | 24.95 | 125.38 | 50.06 | 24.97 | 121.88 |
| 300 | DJ02-13 | 50.10 | 24.91 | 124.61 | 50.14 | 25.01 | 120.43 | DJ02-16 | 50.08 | 25.08 | 126.94 | 50.10 | 25.18 | 122.93 |
| 400 | DJ02-18 | 50.08 | 25.00 | 125.76 | 50.15 | 25.13 | 121.41 | DJ02-19 | 50.10 | 25.05 | 125.14 | 50.19 | 25.14 | 120.62 |
| 500 | DJ02-21 | 50.07 | 24.90 | 121.30 | 50.18 | 25.03 | 116.63 | DJ02-22 | 50.04 | 24.94 | 125.05 | 50.14 | 25.11 | 119.84 |
|
|