Research Article
Damage Characteristics of Uniaxial Compressed Concrete Embedded Different Aging Rubber by 3D Mesoscale Model
Table 4
Elastic modulus and compressive strength of concrete with different contents of rubber.
| Mechanical property | Rubber aggregate content | 3% | 5% | 8% |
| Elastic modulus/GPa | 20.74 | 20.27 | 19.70 | Decrease of elastic modulus | ā | 2.27% | 5.01% | Compressive strength/MPa | 28.25 | 27.49 | 26.36 | Decrease in compressive strength | ā | 2.69% | 6.69% |
|
|