Research Article
Wood Beam Damage Identification Based on the Curvature Mode and Wavelet Transform
Table 2
Condition of damage to the wood beam.
| Working conditions | Damage types | Damage locations (m) | Degrees of damage (%) |
| 0 | Undamaged | — | — |
| 1 | One location damage | 520–560 | 1 | 2 | 520–560 | 2.5 | 3 | 520–560 | 5 | 4 | 520–560 | 10 | 5 | 520–560 | 15 | 6 | 520–560 | 20 | 7 | 1040–1080 | 1 | 8 | 1040–1080 | 2.5 | 9 | 1040–1080 | 5 | 10 | 1040–1080 | 10 | 11 | 1040–1080 | 15 | 12 | 1040–1080 | 20 |
| 13 | Two location damage | 520–560, 1040–1080 | 1 | 14 | 520–560, 1040–1080 | 2.5 | 15 | 520–560, 1040–1080 | 5 | 16 | 520–560, 1040–1080 | 10 | 17 | 520–560, 1040–1080 | 15 | 18 | 520–560, 1040–1080 | 20 |
|
|