Research Article

First-Time Application of Underwater Live Concrete for Economic Retrofitting of Damaged Bridge Piers in Bangladesh

Table 7

Physical properties of cement with standard.

Physical propertiesValueMethod

Fineness99.6%ASTM C184
Normal consistency26.0%ASTM C187 [32]
Initial setting time175 minASTM C191 [33]
Final setting time270 min