Research Article
Determination of Optimized Mix Design of Reactive Powder Concrete
Table 12
Characteristics of Taguchi test designs provided by Minitab.
| RPC mix design | Factors | Characteristics | Cement | Silica sand | Silica powder | Silica fume | Superplasticizer | Water | Compressive strength (MPa) | Water absorption (%) |
| 1 | 890 | 700 | 296 | 187 | 46 | 203 | 143.0 | 1.000 | 2 | 890 | 700 | 296 | 187 | 36 | 198 | 142.3 | 0.981 | 3 | 890 | 700 | 296 | 187 | 46 | 206 | 141.5 | 0.992 | 4 | 890 | 1085 | 261 | 151 | 46 | 203 | 133.0 | 0.960 | 5 | 890 | 1085 | 261 | 151 | 36 | 198 | 134.0 | 1.110 | 6 | 890 | 1085 | 261 | 151 | 46 | 206 | 131.5 | 1.020 | 7 | 890 | 797 | 205 | 188 | 46 | 203 | 142.0 | 0.810 | 8 | 890 | 797 | 205 | 188 | 36 | 198 | 142.5 | 0.762 | 9 | 890 | 797 | 205 | 188 | 46 | 206 | 140.5 | 0.930 | 10 | 629 | 700 | 261 | 188 | 46 | 198 | 131.5 | 1.070 | 11 | 629 | 700 | 261 | 88 | 36 | 206 | 126.0 | 0.830 | 12 | 629 | 700 | 261 | 188 | 46 | 203 | 130.6 | 0.960 | 13 | 629 | 1085 | 205 | 187 | 46 | 198 | 128.0 | 1.011 | 14 | 629 | 1085 | 205 | 187 | 36 | 206 | 125.0 | 0.970 | 15 | 629 | 1085 | 205 | 187 | 46 | 203 | 127.4 | 0.985 | 16 | 629 | 797 | 296 | 151 | 46 | 198 | 129.0 | 0.950 | 17 | 629 | 797 | 296 | 151 | 36 | 206 | 126.5 | 1.110 | 18 | 629 | 797 | 296 | 151 | 46 | 203 | 136.6 | 1.035 | 19 | 897 | 700 | 205 | 151 | 46 | 206 | 140.0 | 0.790 | 20 | 897 | 700 | 205 | 151 | 36 | 203 | 141.2 | 0.757 | 21 | 897 | 700 | 205 | 151 | 46 | 198 | 142.8 | 0.930 | 22 | 897 | 1085 | 296 | 188 | 46 | 206 | 124.2 | 1.086 | 23 | 897 | 1085 | 296 | 188 | 36 | 203 | 123.0 | 0.826 | 24 | 897 | 1085 | 296 | 188 | 46 | 198 | 125.8 | 0.970 | 25 | 897 | 797 | 261 | 187 | 46 | 206 | 146 | 1.000 | 26 | 897 | 797 | 261 | 187 | 36 | 203 | 142.8 | 1.160 | 27 | 897 | 797 | 261 | 187 | 46 | 198 | 146.5 | 1.027 |
|
|