Research Article
Determination of Optimized Mix Design of Reactive Powder Concrete
Table 7
Characteristics of RPC design samples in the experimental program.
| RPC design | Compressive strength (MPa) | Water absorption (%) | Literature value | Test result | Difference (%) | Literature value | Test result | Difference (%) |
| (RPC1) | 132 | 131.5 | 0.38 | 1.04 | 1.050 | 0.96 | (RPC2) | 143 | 142 | 0.70 | 0.98 | 0.985 | 0.51 | (RPC3) | 130 | 130.5 | 0.38 | 0.99 | 0.995 | 0.50 | (RPC4) | 134 | 133 | 0.75 | 0.95 | 0.945 | 0.53 | (RPC5) | 139 | 140 | 0.72 | 1.10 | 1.100 | 0.91 | (RPC6) | 121 | 121.6 | 0.50 | 1.03 | 1.040 | 0.97 | (RPC7) | 125 | 125.8 | 0.64 | 0.79 | 0.794 | 0.50 | (RPC8) | 132 | 131 | 0.76 | 0.75 | 0.756 | 0.80 | (RPC9) | 131 | 130 | 0.76 | 0.93 | 0.926 | 0.43 | (RPC10) | 136 | 136.8 | 0.59 | 1.08 | 1.076 | 0.56 | (RPC11) | 141 | 140.7 | 0.21 | 0.82 | 0.826 | 0.73 | (RPC12) | 138 | 139 | 0.72 | 0.97 | 0.972 | 0.21 | (RPC13) | 144 | 143 | 0.70 | 1.01 | 1.000 | 0.99 |
|
|