Research Article
Potential Use of Scoria as a Cementitious Material for Green Concrete Production
Table 2
Chemical and physical properties of cement used.
| Chemical composition of oxides | Physical properties |
| Oxides | Mean value | Description | Mean value | SiO2 (%) | 20.65 | Residue (%) on 45 µm | 10.50 | Al2O3 (%) | 4.96 | Standard consistency | 28.5 | Fe2O3 (%) | 3.02 | Setting time (minutes) | I.S.T | 155 | CaO (%) | 63.08 | F.S.T | 230 | MgO (%) | 1.42 | Compressive strength (MPa) | 1 day | 11.02 | SO3 (%) | 2.11 | 3 days | 17.40 | LOI | 0.82 | 28 days | 42.63 |
|
|