Research Article
Properties of Carbonated Steel Slag Admixture in the Cementitious System
Table 3
Different carbonation conditions of all samples.
| | 
 |  | Number of sample | Carbonation time | Liquid–solid ratio | Alkali activator |  | 
 |  | T1 | 12 hr | 20% | – |  | T2 | 1 days | 20% | – |  | T3 | 3 days | 20% | – |  | T4 | 7 days | 20% | – |  | T5 | 14 days | 20% | – |  | W0 | 3 days | 0% | – |  | W1 | 3 days | 10% | – |  | W2 | 3 days | 20% | – |  | W3 | 3 days | 30% | – |  | W4 | 3 days | 50% | – |  | W5 | 3 days | 100% | – |  | H1 | 3 days | 50% | NaOH |  | H2 | 7 days | 50% | NaOH |  | H3 | 3 days | 50% | Na2SiO3·9H2O |  | H4 | 7 days | 50% | Na2SiO3·9H2O |  | 
 | 
 |