Research Article
The Effect of Superabsorbent Polymer on Fair-Faced Concrete Performance Based on White Cement
Figure 7
SEM image of 28 days fair-faced concrete: (a) 16x SEM image of group AC; (b) 16x SEM image of group AC-0.2-10; (c) 3000x SEM image of group AC; (d) 3000x SEM image of group AC-0.2-10; (e) 5000x SEM image of group AC; (f) 5000x SEM image of group AC-0.2-10.
| (a) |
| (b) |
| (c) |
| (d) |
| (e) |
| (f) |