Comparative Experimental Study on Strength Properties of Red Clay Modified by Cement and Industrial Solid Waste Powder

Table 4

Weight and additive content of specimens for the UCS tests in different groups.

Additive typeGroup numberDry mass proportion of additive (%)Additive content (g)Weight of mixed specimens (g)

OPC111.57158.14
234.70161.27
357.83164.40
4710.96167.53
5914.09170.66

SS611.57158.14
734.70161.27
857.83164.40
9710.96167.53
10914.09170.66

FA1111.57158.14
1234.70161.27
1357.83164.40
14710.96167.53
15914.09170.66

GGBS1611.57158.14
1734.70161.27
1857.83164.40
19710.96167.53
20914.09170.66