Research Article

Modeling the Influence of Ground-Granulated Blast Furnace Slag on Hydration of Cement

Table 2

Chemical composition of the OPC used in the model (mass%).

Clinker phaseVolume fractionSurface area fraction

C3S0.72290.6689
C2S0.09610.1377
C3A0.12910.1346
C4AF0.03970.0391