Long-Term Performance and Durability of Heat-Treated Alkali-Activated Slag Mortar Containing Silica Fume

Figure 3

The diffraction pattern of the samples at 180 and 360 days of age: (a) SF0.23, (b) SF5.23, (c) SF10.23, (d) SF0.80, (e) SF5.80, (f) SF10.80, and (g) OPC. C, C─S─H; P, portlandite; Ć, calcite; Q, quartz; V, vaterite.