Research Article
Long-Term Performance and Durability of Heat-Treated Alkali-Activated Slag Mortar Containing Silica Fume
Figure 5
SEM images of the heat-cured AAS samples: (a) SF0.80.180 days, (b) SF0.80.360 days, (c) SF5.80.180 days, (d) SF5.80.360 days, (e) SF10.80.180 days, and (f) SF10.80.360 days.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |