Research Article

A Simple Method to Control the Growth of Copper Oxide Nanowires for Solar Cells and Catalytic Applications

Figure 3

XRD pattern of the four samples obtained by the heating rates 1, 2, 5, and 10°C/min. Both copper oxides have been observed to appear by thermal oxidation of copper foils at 550°C for 4 h.