Composition of simulated concrete pore solution (mol/L).
| Serial number | Ca (OH)2 | NaOH | KOH | NaCl |
| pH13.5-CI0 | 0.0303 | 0.202 | 0.505 | | pH13.5-C10.25 | 0.0303 | 0.202 | 0.505 | 0.2525 | pH13.5-C10.5 | 0.0303 | 0.202 | 0.505 | 0.505 | pH13.5-C11.0 | 0.0303 | 0.202 | 0.505 | 1.01 | pH12.5 | 0.002424 | 0.0202 | 0.0505 | | pH12.5 | 0.0002424 | 0.00202 | 0.00505 | |
|
|