Research Article

Laser Beam Welding of AA5052, AA5083, and AA6061 Aluminum Alloys

Figure 8

Fusion zone configuration of alloy AA5083 made using P = 4 kW, S = 6 m/min. (a) Dd =  mm, (b) Dd =  mm.