Research Article
A Novel Sintered Stainless Steel Fiber Felt with Rough Surface Morphologies
Figure 9
Failed sample with 75% porosity sintered at 1200°C for 60 min after tension test. (a) Fracture appearance, (b) SEM image of fracture region, and (c) fractured fiber with necking section.
(a) |
(b) |
(c) |