Research Article
Utilization of Palm Oil Fuel Ash as Binder in Lightweight Oil Palm Shell Geopolymer Concrete
Table 4
Mixture proportions of the OPSGC.
| Mixture | Mix proportions (kg/m3) | POFA | FA | Sand | OPS | AK | Water | SP |
| M1 | 0.0 | 483.8 | 822.5 | 290.3 | 266.1 | 72.6 | 7.3 | M2 | 48.7 | 437.9 | 827.2 | 291.9 | 267.6 | 73.0 | 7.3 | M3 | 97.9 | 391.5 | 831.9 | 293.6 | 269.1 | 73.4 | 7.3 | M4 | 297.0 | 198.0 | 841.5 | 297.0 | 272.2 | 74.3 | 7.4 | M5 | 512.7 | 0.0 | 871.6 | 307.6 | 282.0 | 76.9 | 7.7 | M2-A | 48.7 | 437.9 | 827.2 | 291.9 | 267.6 | 73.0 | 7.3 | M1-2 | 0.0 | 515.6 | 876.5 | 309.4 | 180.5 | 77.3 | 7.7 | M2-2 | 51.9 | 466.8 | 881.8 | 311.2 | 181.6 | 77.8 | 7.8 | M3-2 | 104.4 | 417.5 | 887.2 | 313.1 | 182.7 | 78.3 | 7.8 | M4-2 | 211.3 | 317.0 | 898.1 | 317.0 | 184.9 | 79.2 | 7.9 | M5-2 | 548.5 | 0.0 | 932.5 | 329.1 | 192.0 | 82.3 | 8.2 |
|
|