Research Article
Utilization of Palm Oil Fuel Ash as Binder in Lightweight Oil Palm Shell Geopolymer Concrete
Table 6
Tensile strength of OPSGC.
| Mixture | Tensile strength (MPa) | Splitting tensile | Flexural |
| M1 | 2.12 | 3.55 | M2 | 2.13 | 3.70 | M3 | 2.41 | 3.74 | M4 | 1.62 | 3.11 | M5 | 1.27 | 1.95 | M2-A | 2.03 | 3.31 | M1-2 | 1.66 | 2.65 | M2-2 | 1.62 | 2.55 | M3-2 | 1.53 | 2.36 | M4-2 | 1.25 | 1.93 | M5-2 | 1.17 | 1.85 |
|
|