Review Article

Time Dependent Development of Aluminium Pitting Corrosion

Figure 14

Data and fitted trends for several 6xxx series aluminium alloys exposed to seawater immersion conditions at Esquimalt, BC, Canada. These are different sets of data to those in Figure 13. The changeover to mode 2 occurs at around 2-3 years of exposure. Data from Godard et al. [16].