Review Article
Time Dependent Development of Aluminium Pitting Corrosion
Figure 15
Maximum pit depth trends for low alloy aluminium alloys with oxide stripped off prior to exposure in hard freshwater. Note: horizontal axis is weeks (data from Aziz and Godard [9]).