Review Article
Time Dependent Development of Aluminium Pitting Corrosion
Figure 4
Data for maximum pit depth of aluminium alloys AA5205 and AA5052 exposed in an industrial atmospheric environment showing the trends for pit depth are bimodal. In this case the changeover to mode 2 occurs at about 5 years of exposure. Data from Mattsson and Lindgren [13].