Research Article
Nondestructive Testing of Advanced Concrete Structure during Lifetime
Table 1
The mixture composition.
| | 
 |  | Components | Amount |  | 
 |  | Grained granulated blast furnace slag | 0.45 kg |  | Sodium silicate (water glass) | 0.18 kg |  | Silica sand | 1.35 kg |  | Water | 0.095 L |  | 
 | 
 |