Research Article

Intergranular Corrosion of Low Cr Ferritic Stainless Steel 429 Evaluated by the Optimized Double Loop Electrochemical Potentiokinetic Reactivation Test

Figure 1

Effect of H2SO4 concentration in the DL-EPR test. (a) Influence on values ( mV/min and °C); (b)–(e) micrographs of FSS 429 aging at 550°C for 1 h after test, (b) 0.1 M H2SO4, (c) 0.5 M H2SO4, (d) 1.0 M H2SO4, and (e) 1.5 M H2SO4.
(a)
(b)
(c)
(d)
(e)