Research Article
Durability of Steel Fibres Reinforcement Concrete Beams in Chloride Environment Combined with Inhibitor
Table 2
Composition of concrete.
| | 
 |  | Component | Units | Concrete mix |  | 
 |  | Water | Kg/m3 | 175 |  | Cement (CEMI 32.5 N) | Kg/m3 | 350 |  | w/c ratio | ā | 0.51 |  | Fine aggregate | Kg/m3 | 900 |  | Coarse aggregate | Kg/m3 | 820 |  | Plasticizer BV 40 | Cement weight (%) | 1.2 |  | Target compressive strength | MPa | 30 |  | 
 | 
 |