Research Article
High-Temperature Performance and Multiscale Damage Mechanisms of Hollow Cellulose Fiber-Reinforced Concrete
Table 4
Influence of high temperatures on physical properties of concrete.
| | 
 |  | Concrete series | Temperature (°C) | Holding time (h) | Mass loss ratio (%) | Relative elastic modulus (%) |  | 
 |  | PC | 20 | — | — | — |  | 300 | 2.5 | 3.6 | 77 |  | 4 | 6.2 | 67 |  | 5.5 | 7.6 | 60 |  | 600 | 2.5 | 8.5 | 22 |  | 4 | 11.7 | 17 |  | 5.5 | 12.7 | 14 |  | 
 |  | CFRC | 20 | — | — | — |  | 300 | 2.5 | 3.4 | 82 |  | 4 | 4.8 | 74 |  | 5.5 | 5.6 | 69 |  | 600 | 2.5 | 6.2 | 27 |  | 4 | 6.5 | 25 |  | 5.5 | 7.5 | 24 |  | 800 | 2.5 | 10.5 | 12 |  | 4 | 12.3 | 11 |  | 5.5 | 14.3 | 10 |  | 1050 | 2.5 | 20.5 | 5 |  | 4 | 22.1 | 5 |  | 5.5 | 28.4 | 4 |  | 
 | 
 |