Coercivity field and saturation magnetization of Co-Ni-P films before and after magnetic field annealing.

Co-Ni-P films (Oe) (memu/cm2)

(a) As-deposited84.61179.86
(b) Annealed under 0 T442.58221.60
(c) Annealed under 6 T621.33113.15
(d) Annealed under 12 T471.28149.64