Research Article
Effects of Thermal and Humidity Aging on the Interfacial Adhesion of Polyketone Fiber Reinforced Natural Rubber Composites
Table 5
Chemical composition of the polyketone/NR composite as thermal aging and humidity aging.
| Surface treatment | Chemical composition (%) | Atomic ratio | C | O | O/C |
| Raw | 82.77 | 17.23 | 0.208 |
| Thermal aging | 105°C (8 days) | 79.19 | 20.81 | 0.262 | 125°C (8 days) | 77.74 | 22.26 | 0.286 | 180°C (2 days) | 74.87 | 25.13 | 0.335 | 180°C (8 days) | 74.44 | 25.56 | 0.343 |
| Humidity aging | 99% (500 h) | 83.86 | 16.14 | 0.192 |
|
|