Research Article
Urea Formaldehyde Composites Reinforced with Sago Fibres Analysis by FTIR, TGA, and DSC
Table 2
Results for Sago/UF Sample with different weight fraction analysis by TGA.
| | Weight fraction | Temperature range | Temperature peak | Mass loss | Residue | | (wt%) | (°C) | (°C) | (%) | (%) |
| | Sample D | 62–161 | 75 | 3 | 27 | | 184–539 | 312 | 71 | | Sample E | 60–136 | 74 | 2 | 41 | | 207–534 | 308 | 58 | | Sample F | 55–167 | 76 | 3 | 27 | | 183–569 | 306 | 71 |
|
|