Research Article
Influence of Temperature on Typical Texture Distribution in Primary Recrystallization Matrix of 3% Si CGO Silicon Steel
Table 1
Heat treatment schedule.
| | 
 |  | Representation | Intermediate annealing temperature/°C | Primary recrystallization temperature/°C |  | 
 |  | 800°C + 820°C | 800 | 820 |  | 840°C + 820°C | 840 | 820 |  | 860°C + 820°C | 860 | 820 |  | 800°C + 850°C | 800 | 850 |  | 840°C + 850°C | 840 | 850 |  | 860°C + 850°C | 860 | 850 |  | 
 | 
 |