Research Article
Tests and Models of Hydraulic Concrete Material with High Strength
Table 3
Creep loading test data and numerical simulation results of this paper’s model, sample’s age: 7 days.
| Loading duration increment for recoverable creep/days | Recoverable creep value/10−6/MPa | Fitting parameters | Fitting creep values | Loading duration increment for unrecoverable creep/days | Unrecoverable creep value/10−6/MPa | Fitting parameters | Fitting creep values |
| 3 | 4 | | 2.17 | 3.9 | 90 | 13.1 | | 21.4 | 13.2 | 7 | 6.9 | | 23.5 | 6.7 | 120 | 13.7 | | 0.152 | 13.5 | 10 | 8.2 | | 0.323 | 8.1 | 150 | 14.1 | | 0.274 | 13.9 | 15 | 9.1 | | 2.835 | 9 | 200 | 14.5 | | 0.0395 | 14.6 | 30 | 10.4 | | 19.84 | 10.2 | | | | | | 45 | 11.3 | | 0.27 | 11.2 | | | | | | 60 | 12.1 | | 0.0136 | 12 | | | | | |
|
|