Research Article

Microstructure and Mechanical Behavior of Hot Pressed Cu-Sn Powder Alloys

Figure 8

The stress-strain curves for the heat-treated (a) 90% Cu-10% Sn and 85% Cu-10% Sn-5% C and (b) 80% Cu-10% Sn-10% Pb and 90% Cu-10% Pb alloys.
(a)
(b)