Research Article
Surface Corrosion and Microstructure Degradation of Calcium Sulfoaluminate Cement Subjected to Wet-Dry Cycles in Sulfate Solution
Figure 2
Surface change of CSA cement 0.50 w/c specimen under wet-dry cycles in 5% Na2SO4 solution.
(a) 18 cycles |
(b) 22 cycles |
(c) 25 cycles |
(d) 31 cycles |
(e) 39 cycles |
(f) 41 cycles |
(g) 43 cycles |