Research Article

Surface Corrosion and Microstructure Degradation of Calcium Sulfoaluminate Cement Subjected to Wet-Dry Cycles in Sulfate Solution

Figure 4

Surface change of CSA cement specimens under wet-dry cycles in 5% Na2SO4 solution.
(a) 0.50 w/c, 46 cycles
(b) 0.40 w/c, 46 cycles
(c) 0.30 w/c, 46 cycles
(d) 0.30 w/c, 119 cycles