Research Article

Surface Corrosion and Microstructure Degradation of Calcium Sulfoaluminate Cement Subjected to Wet-Dry Cycles in Sulfate Solution

Figure 7

SAC 0.50 w/c specimen subjected to 46 wet-dry cycles in 3% Na2SO4 + 1.80% MgSO4 solution.
(a) Surface change
(b) SEM image