Surface Corrosion and Microstructure Degradation of Calcium Sulfoaluminate Cement Subjected to Wet-Dry Cycles in Sulfate Solution
Figure 8
CSA cement 0.50 w/c specimen subjected to 46 wet-dry cycles in 3% Na2SO4 + 1.80% MgSO4 + 3% NaCl solution.
(a) Surface change |
(b) SEM image |