Research Article

Combined Effects of Sustained Loads and Wet-Dry Cycles on Durability of Glass Fiber Reinforced Polymer Composites

Figure 5

Micrographs of the longitudinal section (×50) of the unstressed specimens: (a) unconditioned specimen; (b) WWD0 after 60 WD cycles; (c) SWD0 after 60 WD cycles; and (d) WWD0 after 180 WD cycles.
(a)
(b)
(c)
(d)