Research Article

Investigation of the Scanning Microarc Oxidation Process

Figure 10

Plot showing coating thickness as a function of cathode travel speed for A356 alloy using a Na2SiO3 and NaOH electrolyte solution (AC1 and 5 mm interelectrode gap).