Research Article
Investigation of the Scanning Microarc Oxidation Process
Figure 2
Photographs showing SMAO discharge distributions and diameters taken at (a) 10 s, mm; (b) 2 min, mm; (c) 3 min, mm; (d) 5 min, mm; (e) 10 min, mm; (f) 15 min, mm.
| (a) |
| (b) |
| (c) |
| (d) |
| (e) |
| (f) |