Research Article
Enhancing Ductility of 1045 Nanoeutectic Steel Prepared by Aluminothermic Reaction through Annealing at 873 K
Figure 7
Bright field TEM micrographs of the pearlite in 1045 carbon steel without (a) and with annealing at 873 K (600°C) for 2 h (b), 4 h (c), and 6 h (d).
(a) |
(b) |
(c) |
(d) |