Corrosion and Strength Behaviors in Prestressed Tendon under Various Tensile Stress and Impressed Current Conditions
Table 1
The entire procedure for loading and corrosion tests.
| | 
 |  | Step | Action | Related photos |  | 
 |  | 1st | Installation of steel frame and tendon setup |  |  | 
 |  | 2nd | Preparation of 3.5% NaCl solution and saturation |  |  | 
 |  | 3rd | Installation of bearing plate, barrel, and wedge |  |  | 
 |  | 4th | Welding of strand and wire/attachment of gauge |  |  | 
 |  | 5th | Prestressing to designed level (0%, 20%, 40%, and 60% of the ultimate loading) |  |  | 
 |  | 6th | Performing ICM with 20 V for 1 day |  |  | 
 |  | 7th | Loading to failure |  |  | 
 |  | 8th | Measurement of corroded weight |  |  | 
 | 
 |