Physical properties of SK-90 and Sasobit modified asphalt binder.
| Asphalt binders | 25°C penetration (0.1 mm) | 15°C ductility (cm) | Softening point (°C) | 60°C dynamic viscosity (Pa·s) | After RTFOT | Mass loss (%) | Penetration ratio (%) | 10°C ductility (cm) |
| SK-90 | 79 | >100 | 52.8 | 141.2 | −0.113 | 61.3 | 10.4 | Sasobit-modified asphalt binder | 54 | >100 | 75.9 | 953.7 | 0.198 | 58.4 | 5.2 |
|
|