Plasticity Improvement of Ball-Spun Magnesium Alloy Tube Based on Stress Triaxiality
Table 2
Average stress triaxial value for different process parameters.
| No. | R | Δt | f | TRIAX | No. | R | Δt | f | TRIAX | No. | R | Δt | f | TRIAX |
| 1 | 2.5 | 0.2 | 0.2 | −0.7413 | 13 | 2.5 | 0.3 | 0.1 | −0.1733 | 25 | 4.5 | 0.3 | 0.2 | −0.8001 | 2 | 3.5 | 0.2 | 0.2 | −0.9252 | 14 | 2.5 | 0.3 | 0.15 | −0.4531 | 26 | 4.5 | 0.4 | 0.2 | −0.6585 | 3 | 4 | 0.2 | 0.2 | −0.8034 | 15 | 2.5 | 0.3 | 0.25 | −0.4681 | 27 | 4.5 | 0.5 | 0.2 | −0.6274 | 4 | 4.5 | 0.2 | 0.2 | −0.7574 | 16 | 2.5 | 0.3 | 0.3 | −0.2836 | 28 | 3 | 0.1 | 0.2 | −0.6487 | 5 | 2.5 | 0.2 | 0.3 | −0.6020 | 17 | 2.5 | 0.2 | 0.1 | −0.4014 | 29 | 3 | 0.2 | 0.2 | −1.0312 | 6 | 3.5 | 0.2 | 0.3 | −0.7252 | 18 | 2.5 | 0.2 | 0.15 | −0.6340 | 30 | 3 | 0.4 | 0.2 | −0.5260 | 7 | 4 | 0.2 | 0.3 | −0.5834 | 19 | 2.5 | 0.2 | 0.25 | −0.7329 | 31 | 3 | 0.5 | 0.2 | −0.4594 | 8 | 4.5 | 0.2 | 0.3 | −0.5074 | 20 | 3 | 0.2 | 0.1 | −0.5552 | 32 | 3 | 0.1 | 0.3 | −0.5487 | 9 | 2.5 | 0.3 | 0.2 | −0.5699 | 21 | 3 | 0.2 | 0.15 | −0.8883 | 33 | 3 | 0.3 | 0.3 | −0.5886 | 10 | 3 | 0.3 | 0.2 | −0.8416 | 22 | 3 | 0.2 | 0.25 | −0.9686 | 34 | 3 | 0.4 | 0.3 | −0.3063 | 11 | 3.5 | 0.3 | 0.2 | −0.7552 | 23 | 3 | 0.2 | 0.3 | −0.8766 | 35 | 3 | 0.5 | 0.3 | −0.2050 | 12 | 4 | 0.3 | 0.2 | −0.7634 | 24 | 4.5 | 0.1 | 0.2 | −0.4416 | | | | | |
|
|