Research Article
Mechanical Properties Improvement Mechanism of Silica Fume-Modified Ultrafine Cement Used to Repair Pavement Microcracks
| Number | Tensile shear bonding strength | Bending tensile bonding strength | Avg (MPa) | Average cementation ratio | Max (MPa) | Maximum cementation ratio | Avg (MPa) | Average cementation ratio | Max (MPa) | Maximum cementation ratio |
| GC0 | 0.0458 | 1.00 | 0.0625 | 1.00 | 3.48 | 1.00 | 3.55 | 1.00 | GC1 | 0.1229 | 2.68 | 0.1500 | 2.40 | 3.21 | 1.00 | 3.65 | 1.00 | GC2 | 0.2141 | 4.67 | 0.2625 | 4.20 | 3.37 | 0.92 | 3.78 | 1.03 | GC3 | 0.3938 | 8.60 | 0.4313 | 6.90 | 3.75 | 0.97 | 4.11 | 1.06 | GC4 | 0.3792 | 8.28 | 0.6625 | 10.60 | 3.73 | 1.08 | 4.03 | 1.16 | GC5 | 0.3063 | 6.69 | 0.3375 | 5.40 | 3.59 | 1.07 | 3.99 | 1.14 |
|
|