Research Article

Study on the Performance of High-Speed Rail Damage of Four Different Materials

Table 1

Mass fraction of sample materials.

No. (%)
CSiMnPSV

PD3 quenched0.7930.7120.7710.0300.0300.120
PD3 hot rolled0.7930.7120.7710.0220.0140.070
U71Mn quenched0.7360.2821.4000.0200.0300.040
U71Mn hot rolled0.7360.2821.4000.0200.0300.040